Notice: Function _load_textdomain_just_in_time was called incorrectly. Translation loading for the wordpress-seo domain was triggered too early. This is usually an indicator for some code in the plugin or theme running too early. Translations should be loaded at the init action or later. Please see Debugging in WordPress for more information. (This message was added in version 6.7.0.) in /var/www/html/wp-includes/functions.php on line 6260 Extrusion Bonded Laminates for Absorbent Articles - Nonwovens Industry
Patents

Extrusion Bonded Laminates for Absorbent Articles

Receiving a U.S. patent is an absorbent article comprising:  a topsheet; an outer cover; an absorbent core disposed between the topsheet and outer cover. The outer cover comprises an extrusion bonded laminate, the extrusion bonded laminate comprising:
– a multi-layer coextruded elastomeric film with a core layer, a first outer layer, and a second outer layer, wherein the core layer is between the first and second outer layers;
– a nonwoven consisting of fibers and/or filaments;
The first outer layer is non-adhesively joined to the nonwoven via extrusion coating, such that the first outer layer is a tie layer between the core layer and the nonwoven. The second outer layer is non-adhesively joined to the core layer, such that the second outer layer is a skin layer; wherein the first and second outer layers comprise polyolefin elastomers (POEs) and the first and second outer layers comprise a blend of two ethylene-rich copolymers. Ethylene is between 10% and 97%;  wherein the first outer layer and the second outer layer have the same composition; wherein the extrusion bonded laminate is mechanically activated using intermeshing gears; wherein the outer cover is elastic at 50% engineering strain and is substantially free from pinholes; wherein the nonwoven has a high chemical affinity for the first outer layer; wherein the first outer layer has a low chemical affinity for the core layer; wherein the multi-layer coextruded elastomeric film has a basis weight from 1 gsm to 25 gsm; and wherein the laminate bond strength is from 1 N/cm to 3.5 N/cm.

Add us as a preferred source on Google

Get the latest Nonwovens Industry news, insights and analysis in your Google Search and AI experiences.

Keep Up With Our Content. Subscribe To Nonwovens Industry Newsletters